speċifikazzjoni tal-magna tal-iwweldjar bil-fużjoni tar-ras
DN (mm) | Ħxuna e (mm) | P2 (MPa) | Pressjoni=għoli tal-projezzjoni P1 h (mm) | Pressjoni ≈ P Drag il-ħin ta 'assorbiment tas-sħana t2(s) | Ħin tal-bidla t3(s) |
t4(s) | Pressjoni=skeda tat-tkessiħ P15 (min) |
75 | 6.8 | 219/S2 | 1.0 | 68 | ≤5 | <6 | ≥10 |
90 | 8.2 | 315/S2 | 1.5 | 82 | ≤6 | <7 | ≥11 |
110 | 10.0 | 471/S2 | 1.5 | 100 | ≤6 | <7 | ≥14 |
125 | 11.4 | 608/S2 | 1.5 | 114 | ≤6 | <8 | ≥15 |
140 | 12.7 | 763/S2 | 2.0 | 127 | ≤8 | <8 | ≥17 |
160 | 14.5 | 996/S2 | 2.0 | 145 | ≤8 | <9 | ≥19 |
180 | 16.4 | 1261/S2 | 2.0 | 164 | ≤8 | <10 | ≥21 |
200 | 18.2 | 1557/S2 | 2.0 | 182 | ≤8 | <11 | ≥23 |
225 | 20.5 | 1971/S2 | 2.5 | 205 | ≤10 | <12 | ≥26 |
250 | 22.7 | 2433/S2 | 2.5 | 227 | ≤10 | <13 | ≥28 |
280 | 25.5 | 3052/S2 | 2.5 | 255 | ≤12 | <14 | ≥31 |
315 | 28.6 | 3862/S2 | 3.0 | 286 | ≤12 | <15 | ≥35 |
355 | 32.3 | 4903/S2 | 3.0 | 323 | ≤12 | <17 | ≥39 |
400 | 36.4 | 6228/S2 | 3.0 | 364 | ≤12 | <19 | ≥44 |
注
1, Il-parametri ta 'hawn fuq huma bbażati fuq it-temperatura ambjentali ta' 20 ℃.
2, It-temperatura tal-wiċċ tal-hot plate: 210 ± 10 ℃ għal PE80 u 225 ± 10 ℃ għal PE100.
3, S2 hija l-erja effettiva totali tal-pistun fiċ-ċilindru idrawliku tal-welder (mm2), li hija pprovduta mill-manifattur tal-welder.
It-tags Popolari: butt fużjoni magna iwweldjar, iċ-Ċina, fornituri, manifatturi, fabbrika, prezz, għall-bejgħ